Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 260 kJ/m² | 124 ft-lb/in² | |
LyondellBasell Lupolen® 4261 A HDPE, Blow Molding Grade Easy-to-process bow molding grade for technical containers such as fuel tanks, petrol filler inlets, expansion tanks, horticultural spray tanks, tanks for lawnmowers, disposable containers (up to 10.. |