Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 263 kJ/m² | 125 ft-lb/in² | ASTM D1822 |
ExxonMobil HD 9856BA Blow Molding Resin
(discontinued **) HD 9856BA is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856BA exhibit a unique combination of stiffness and environmental stress cracki.. |