Material Notes:
HD 9856BA is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856BA exhibit a unique combination of stiffness and environmental stress cracking resistance. These properties, coupled with excellent processability on both continuous and intermittent equipment, afford significant lightweighting and/or fast cycling potential in many applications. HD 9865BA contains an antistat which may be used in contact with limited types of food.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Bulk Density 0.585 g/cc
0.0211 lb/in³
Density 0.957 g/cc
0.0346 lb/in³
ASTM D4883
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
ASTM D1693
Melt Flow 0.46 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.46 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 24.1 MPa
3500 psi
ASTM D638
Tensile Strength, Yield 30.3 MPa
4400 psi
ASTM D638
Elongation at Break 1100 %
1100 %
ASTM D638
Elongation at Yield 7.5 %
7.5 %
ASTM D638
Flexural Modulus 1.48 GPa
215 ksi
1% Secant; ASTM D790
Tensile Impact Strength 263 kJ/m²
125 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Brittleness Temperature >= -76.1 °C
>= -105 °F
ASTM D746
Descriptive Properties Value Comments
Features Thermal Stabilizer