Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 589 kJ/m² | 280 ft-lb/in² | ASTM Data |
Styron CALIBRE™ 200 6 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Tensile Impact Strength | 588 kJ/m² | 280 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ 200-6 Polycarbonate Resin Overview: CALIBREâ„¢ 200-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Tensile Impact Strength | 588 kJ/m² | 280 ft-lb/in² | ASTM D1822, Type S |
Styron CALIBREâ„¢ 201-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Impact Strength | 588 kJ/m² | 280 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ 201-6 Polycarbonate Resin Overview: CALIBREâ„¢ 201-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Tensile Impact Strength | 588 kJ/m² | 280 ft-lb/in² | ASTM D1822 |
Styron CALIBRE™ 2060-6 Polycarbonate Resin Overview: CALIBRE™ 2060-6 polycarbonate resin is used in medical applications involving steam or ethylene oxide sterilization – through suitability for use in these applications is depende.. |
|||
Tensile Impact Strength | 589 kJ/m² | 280 ft-lb/in² | ASTM Data |
Styron CALIBRE™ 300 6 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Tensile Impact Strength | 588 kJ/m² | 280 ft-lb/in² | ASTM D1822, Type S |
Styron CALIBREâ„¢ 301-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Impact Strength | 588 kJ/m² | 280 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ 301-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet applic.. |
|||
Tensile Impact Strength | 588 kJ/m² | 280 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ 301V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 301V-6 Polycarbonate resins offer exceptional impact resistance and heat distortion resistance, and meets UL94 V-2 rating. CALIBRE 301V-6 contains a mold release agent and is.. |
|||
Tensile Impact Strength | 588 kJ/m² | 280 ft-lb/in² | ASTM D1822, Type S |
Styron CALIBREâ„¢ IM 401-18 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Impact Strength | 589 kJ/m² | 280 ft-lb/in² | ASTM Data |
Styron CALIBRE™ MEGARAD 2080 10 Polycarbonate, Gamma Radiation Resistant CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g.. |
|||
Tensile Impact Strength | 588 kJ/m² | 280 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ 300-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity as high melt strength for blow molding and sheet applications. .. |
|||
Tensile Impact Strength | 588 kJ/m² | 280 ft-lb/in² | ASTM D1822, Type S |
Styron CALIBREâ„¢ 302-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Impact Strength | 588 kJ/m² | 280 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ 302-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Tensile Impact Strength | 588 kJ/m² | 280 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ 302V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 302V-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity (for tinted/transparent colors), and is available in both tint.. |
|||
Tensile Impact Strength | 588 kJ/m² | 280 ft-lb/in² | ASTM D1822, Type S |
Styron CALIBREâ„¢ 303-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Impact Strength | 588 kJ/m² | 280 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ 303V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 303V-6 Polycarbonate resins offer exceptional impact resistance and heat distortion resistance, and meets UL94 V-2 rating. CALIBRE 303V-6 contains a mold release agent, a UV .. |
|||
Tensile Impact Strength | 588 kJ/m² | 280 ft-lb/in² | ASTM D1822 |
Styron CALIBREâ„¢ IM 401-18 Polycarbonate Resin Overview: CALIBREâ„¢ IM 401-18 Impact Modified Polycarbonate resin is available in opaque formulations that offer benefits ranging from superior low temperature impact strength to easy process wi.. |