Mechanical Properties Metric English Comments
Tensile Impact Strength 340 kJ/m²
162 ft-lb/in²
Solvay Specialty Polymers Veradel® A-100, A-200, A-300 Polyethersulfone  (discontinued **)
For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N..
Tensile Impact Strength 340 kJ/m²
162 ft-lb/in²
ASTM D1822S
DuPont™ Surlyn® 7930 Ionomer Resin, Lithium
Surlyn® 7930 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne..
Tensile Impact Strength 340 - 1320 kJ/m²
162 - 628 ft-lb/in²
Average value: 837 kJ/m² Grade Count:27
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..