Tensile Impact Strength
95.5
kJ/m²
45.5
ft-lb/in²
ASTM D-1822
Axiall 2512 Rigid PVC, Extrusion
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.