Mechanical Properties Metric English Comments
Tensile Impact Strength 460 kJ/m²
219 ft-lb/in²
ASTM D1822S
DuPont™ Surlyn® 7940 Ionomer Resin, Lithium
Surlyn® 7940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne..