Polymer Property : Tensile Impact Strength = 480 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 480 kJ/m²
228 ft-lb/in²
ASTM D1822
NOVA Chemicals Novapol® HB-W747-A HDPE Extrusion Resin
Molded Plaque Properties. Features: High molecular weight, excellent ESCR, impact strength, easy processing.Data provided by the manufacturer.
Tensile Impact Strength 480 kJ/m²
228 ft-lb/in²
23°C; ASTM D-1822
ExxonMobil Iotek® 7030 Zinc Ionomer Molding/Extrusion Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas..