Material Notes:
Molded Plaque Properties. Features: High molecular weight, excellent ESCR, impact strength, easy processing.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.947 g/cc
0.0342 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
F50, Condition A OR B, ASTM D1693, 100% Igepal
Melt Flow 8.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa
3340 psi
ASTM D638
Elongation at Break 830 %
830 %
ASTM D638
Flexural Modulus 1.20 GPa
174 ksi
ASTM D790
Izod Impact, Notched 4.00 J/cm
7.49 ft-lb/in
Notched/Unnotched not specified; ASTM D256
Tensile Impact Strength 480 kJ/m²
228 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D696
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F