Polymer Property : Tensile Impact Strength = 75.0 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 158 kJ/m²
75.0 ft-lb/in²
ASTM D1822
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet
High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines..
Tensile Impact Strength 158 kJ/m²
75.0 ft-lb/in²
ASTM D-1822
Axiall 5055 Rigid PVC, Extrusion, White
Georgia Gulf 5055 White is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical ResistantOutdoor..
Tensile Impact Strength 158 kJ/m²
75.0 ft-lb/in²
ASTM D-1822
Axiall 7045 Rigid PVC, Extrusion
Georgia Gulf 7045 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityDimen..
Tensile Impact Strength 158 kJ/m²
75.0 ft-lb/in²
ASTM D-1822
Axiall 7181 Rigid PVC, Extrusion
Georgia Gulf 7181 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: WeatherabilityImpact StrengthDimensional StabilityFlame Ret..
Tensile Impact Strength 158 kJ/m²
75.0 ft-lb/in²
ASTM D-1822
Axiall 7555 Rigid PVC, Extrusion, Natural
Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn..
Tensile Impact Strength 158 kJ/m²
75.0 ft-lb/in²
ASTM D-1822
Axiall 7555 Rigid PVC, Extrusion, White
Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn..
Tensile Impact Strength 158 kJ/m²
75.0 ft-lb/in²
ASTM D-1822
Axiall 7768 Rigid PVC, Extrusion
Georgia Gulf 7768 is a general purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityDimen..
Tensile Impact Strength 158 kJ/m²
75.0 ft-lb/in²
ASTM D-1822
Axiall 8258 Rigid PVC, Extrusion
Georgia Gulf 8258 is a special purpose rigid PVC for film and food grade sheet compound. It has been used where packages are manufactured to FDA guidelines.Information provided by Georgia GulfGeorg..
Tensile Impact Strength 158 kJ/m²
75.0 ft-lb/in²
ASTM D-1822
Axiall 5055 Rigid PVC, Extrusion, Natural
Georgia Gulf 5055 is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical RetardantInformation p..