Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 94.5 kJ/m² | 45.0 ft-lb/in² | Type S; ASTM D1822 |
Chase Plastics CP Pryme® AC125 Acetal Copolymer, 25% Glass Fiber Reinforced Features: Glass fiber reinforcedAlkali resistantGood chemical resistanceGood dimensional stabilityFatigue resistantLow frictionGrease resistantLow moisture absorptionOil resistantResilientHigh rigid.. |
|||
Tensile Impact Strength | 94.5 kJ/m² | 45.0 ft-lb/in² | ASTM D-1822 |
Axiall HHW-191 Rigid PVC, Extrusion Georgia Gulf HHW-191 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Excellent WeatherabilityImpact Strength & ToughnessColorabilityChemic.. |
|||
Tensile Impact Strength | 94.5 kJ/m² | 45.0 ft-lb/in² | ASTM D1822 |
ExxonMobil Paxon™ BA7794 Sheet Extrusion and Blow Molding Resin
(discontinued **) BA7794 is a 25% talc-filled, high molecular weight, high density polyethylene. This color match-able material has been specifically developed as a cost effective resin for applications which requir.. |