Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 2270 MPa
329000 psi
Arkema Group Orgalloy® RS 6600 Nylon 66 Alloy, Rigid Grade (Conditioned)
RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie..
Tensile Creep Modulus, 1 hour 2270 MPa
329000 psi
ISO 899-1
Arkema Group Orgalloy® RS 6600 Polyamide 6.6 Alloy
Polyamide Alloy, Rigid grade, Nylon 6.6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group