Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 420 MPa
60900 psi
Arkema Group Orgalloy® LT 5050 Flexible Nylon Alloy (Conditioned)
Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good ..
Tensile Creep Modulus, 1 hour 420 MPa
60900 psi
ISO 899-1
Arkema Group Orgalloy® LT 5050 Polyamide Alloy
Polyamide Alloy, Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
Tensile Creep Modulus, 1 hour 420 - 1520 MPa
60900 - 220000 psi
Average value: 938 MPa Grade Count:11
Overview of materials for Nylon, Flexible Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri..
Tensile Creep Modulus, 1 hour 420 MPa
60900 psi
ISO 899-1
Arkema Group Orgalloy® LT 5050 ES Polyamide Alloy
Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group
Tensile Creep Modulus, 1 hour 420 MPa
60900 psi
Arkema Group Orgalloy® LT 5050ES Flexible Nylon Alloy (Conditioned)
Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good ..
Tensile Creep Modulus, 1 hour 420 MPa
60900 psi
Arkema Group Orgalloy® LT 5050T Flexible Nylon Alloy (Conditioned)
Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good ..