Tensile Creep Modulus, 1 hour 400 MPa
58000 psi
LyondellBasell Lupolen® 5021 D HDPE, Blow Molding Grade
Easy flow, blow molding grade for small containers (up to 5 l), bottles for surface-active substances, household chemicals, laundry and dishwashing detergents, sanitary cleaners, cosmetics and pharm..
Tensile Creep Modulus, 1 hour 400 MPa
58000 psi
LyondellBasell Lupolen® 5261 Z HI HDPE
Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Tensile Creep Modulus, 1 hour 400 MPa
58000 psi
LyondellBasell Lupolen® 5261 ZS HDPE, Blow Molding Grade
Relatively high viscosity blow molding grade (similar to Lupolen 5261 Z), but more resistant to stress cracking) for rigid, stackable and highly shock resistant containers for packaging all types of..
Tensile Creep Modulus, 1 hour 400 - 570 MPa
58000 - 82700 psi
Average value: 465 MPa Grade Count:4
Overview of materials for High Density Polyethylene (HDPE), Injection Molded