Modulus of Elasticity 2.76 GPa
400 ksi
ASTM D638
Technetics Group Amicon™ Nylon 6/66  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Modulus of Elasticity 2.76 - 7.50 GPa
400 - 1090 ksi
Average value: 4.12 GPa Grade Count:4
Overview of materials for Nylon 6, Stainless Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o..
Modulus of Elasticity 2.76 - 15.2 GPa
400 - 2200 ksi
Average value: 6.95 GPa Grade Count:59
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Modulus of Elasticity 2.76 - 4.14 GPa
400 - 600 ksi
Average value: 3.22 GPa Grade Count:6
Overview of materials for Nylon 11 with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ..
Modulus of Elasticity 2.76 GPa
400 ksi
Secant; ASTM D882
Specialty Coating Systems Parylene C Poly (P-Xylylene) Coating
Parylene C is a polymer of para-xylylene modified by the substitution of a chlorine atom for one of the aromatic hydrogen atoms. Parylene C has a useful combination of electrical and physical proper..
Modulus of Elasticity 2.76 - 6.89 GPa
400 - 999 ksi
ERG Aerospace Duocel® Silicon Carbide Foam
Silicon Carbide (SiC) foam is a porous, open-celled structure made from an interconnected lattice of ceramic ligaments. The pattern of cells and ligaments repeats regularly throughout the entirety o..
Modulus of Elasticity 2.76 GPa
400 ksi
IPC TM-650 2.4.18.3
Arlon AD255C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs
For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.55) with Tighter Toleran..
Modulus of Elasticity 2.76 GPa
400 ksi
ASTM D412
Aaron Industries AAROPRENE® ATPR ECATPR2040 Black Thermoplastic SEBS Rubber
AAROPRENE® ATPR 2000 Series Elastomeric CompoundFeatures: A black, thermoplastic SEBS Rubber compound specifically designed for the injection molding of industrial gaskets.
Modulus of Elasticity 2.76 GPa
400 ksi
ASTM D638
Technetics Group Amicon™ Acetal Copolymer  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Modulus of Elasticity 2.76 GPa
400 ksi
ASTM D882
Mitsui AURUM® PL450C Polyimide  (discontinued **)
AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURU..
Modulus of Elasticity 2.76 - 5.52 GPa
400 - 800 ksi
Average value: 4.21 GPa Grade Count:5
Overview of materials for Polypropylene with Glass Fiber + PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va..