Mechanical Properties Metric English Comments
Modulus of Elasticity 2.41 - 4.14 GPa
350 - 600 ksi
Average value: 3.58 GPa Grade Count:17
Overview of materials for Nylon 66, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri..
Modulus of Elasticity 3.10 - 4.14 GPa
450 - 600 ksi
Average value: 3.54 GPa Grade Count:11
Overview of materials for Nylon 612, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of..
Modulus of Elasticity 2.76 - 4.14 GPa
400 - 600 ksi
Average value: 3.22 GPa Grade Count:6
Overview of materials for Nylon 11 with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ..