Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 0.0400 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.00650 - 0.0400 GPa
0.943 - 5.80 ksi
Average value: 0.0203 GPa Grade Count:5
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
Modulus of Elasticity 0.0300 - 0.0400 GPa
4.35 - 5.80 ksi
TM-019E
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets
Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc...
Modulus of Elasticity 0.0300 - 0.0400 GPa
4.35 - 5.80 ksi
TM-019E
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets
Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc...