Modulus of Elasticity 0.680 GPa
98.6 ksi
ISO 527
GEHR Plastics PE-UHMW Polyethylene, Ultra High Molecular Weight
The ultra high molecular weight Polyethylene has a high abrasion resistance and a high toughness at the same time. The chemical and the crack resistance are optimized in comparison to the standard P..
Modulus of Elasticity 0.680 - 3.60 GPa
98.6 - 522 ksi
Average value: 1.47 GPa Grade Count:40
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..