Polymer Property : Modulus of Elasticity = 3.60 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 1.30 - 3.60 GPa

@Temperature 60.0 - 120 °C
189 - 522 ksi

@Temperature 140 - 248 °F
Average value: 2.73 GPa Grade Count:1
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Modulus of Elasticity 1.72 - 3.60 GPa
250 - 522 ksi
Average value: 2.86 GPa Grade Count:14
Overview of materials for Acrylic, Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o..
Modulus of Elasticity 0.680 - 3.60 GPa
98.6 - 522 ksi
Average value: 1.47 GPa Grade Count:40
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..