Polymer Property : Modulus of Elasticity = 0.745 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.745 GPa
108 ksi
Molded Sample 2% Secant Modulus
Dow HDPE 10462N High Density Polyethylene
DOW HDPE 10462N resin is a narrow molecular weight distribution polymer designed to offer good stress crack resistance and impact strength with excellent rigidity. This resin has good processability..