Material Notes:
DOW HDPE 10462N resin is a narrow molecular weight distribution polymer designed to offer good stress crack resistance and impact strength with excellent rigidity. This resin has good processability over a wide range of molding conditions. Typical applications are industrial shipping containers, cases/crates etc. It complies with FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.962 g/cc
0.0348 lb/in³
Viscosity 80000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
80000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
180000 cP

@Shear Rate 1000 1/s,
Temperature 190 °C
180000 cP

@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
260000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
260000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Melt Flow 10 g/10 min

@Load 2.16 kg
10 g/10 min

@Load 4.76 lb
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 12.4 MPa
1800 psi
Tensile Strength, Yield 23.4 MPa
3390 psi
Elongation at Break 1000 %
1000 %
Modulus of Elasticity 0.745 GPa
108 ksi
Molded Sample 2% Secant Modulus
Flexural Modulus 1.08 GPa
157 ksi
Izod Impact Resistance 9.61 J/cm²
45.7 ft-lb/in²
Thermal Properties Metric English Comments
Vicat Softening Point 128 °C
262 °F