Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.827371 - 1.86158 GPa @Temperature 60.0 - 149 °C |
120.002 - 270.004 ksi @Temperature 140 - 300 °F |
Average value: 1.59 GPa Grade Count:3 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Modulus of Elasticity | 0.827371 - 0.827371 GPa @Temperature 60.0 - 60.0 °C |
120.002 - 120.002 ksi @Temperature 140 - 140 °F |
Average value: 0.827 GPa Grade Count:1 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |