Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.425 GPa | 206.7 ksi | 50% RH |
Murtfeldt Murylon® B Nylon 6 Murylon® B natural has the best impact resistance of all Murylon materials. This material is especially suited for use in machine construction thanks to an excellent combination of mechanical prope.. |