Polymer Property : Modulus of Elasticity = 1.87 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 1.87 - 2.90 GPa
271 - 420 ksi
Average value: 2.36 GPa Grade Count:21
Overview of materials for PVC/Acrylic Alloy
This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate ..