Mechanical Properties Metric English Comments
Modulus of Elasticity 7.20 - 16.0 GPa

@Temperature 60.0 - 150 °C
1040 - 2320 ksi

@Temperature 140 - 302 °F
Average value: 11.7 GPa Grade Count:2
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Modulus of Elasticity 7.20 GPa
1040 ksi
ASTM D638
Toyobo T-750 Nylon, Painting Grade
Key Feature: Glass fiber and mineral reinforced, high heat distortion gradesInformation provided by Toyobo Co., Ltd
Modulus of Elasticity 7.20 GPa
1040 ksi
When curved
Voloknohim PA-SV30 Glass and Mineral Filled
Information provided by Voloknokhim
Modulus of Elasticity 7.20 GPa
1040 ksi
ISO 527-1/-2
BASF Ultramid® B3WG7 BK 00564 35% Glass Filled PA6 (Conditioned)
Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF
Modulus of Elasticity 7.20 GPa
1040 ksi
ISO 527-1/-2
BASF Ultramid® S3WG7 Balance 35% Glass Filled PA 610 (Conditioned)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..
Modulus of Elasticity 7.20 GPa
1040 ksi
ISO 527
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Conditioned)
Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability.
Modulus of Elasticity 7.20 GPa
1040 ksi
ISO 527-1/-2
BASF Ultramid® A3WG6 BK 00564 30% Glass Filled PA66 (Conditioned)
Description: 30% glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of high stiffness and dimensional stability such as lamp socket housings, f..
Modulus of Elasticity 7.20 GPa
1040 ksi
ISO 527-1/-2
BASF Ultramid® A3HG6 Balance 30% Glass Filled PA 66/610 (Conditioned)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..