Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 111 GPa | 16100 ksi | |
Schott N-LASF40 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 111 GPa | 16100 ksi | |
Schott N-LAF33 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 111 GPa | 16100 ksi | Alternate report from Timet |
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 538°C High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
Modulus of Elasticity | 111 GPa | 16100 ksi | |
Schott N-LAK14 Glass Information Provided by SCHOTT North America, Inc. |