Polymer Property : Modulus of Elasticity = 16100 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 111 GPa
16100 ksi
Schott N-LASF40 Glass
Information Provided by SCHOTT North America, Inc.
Modulus of Elasticity 111 GPa
16100 ksi
Schott N-LAF33 Glass
Information Provided by SCHOTT North America, Inc.
Modulus of Elasticity 111 GPa
16100 ksi
Alternate report from Timet
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 538°C
High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess..
Modulus of Elasticity 111 GPa
16100 ksi
Schott N-LAK14 Glass
Information Provided by SCHOTT North America, Inc.