Modulus of Elasticity 7.65 - 24.1 GPa
1110 - 3500 ksi
Average value: 15.5 GPa Grade Count:4
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and..