Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic/Polycarbonate Alloy, Carbon Fiber Filler , Polycarbonate (PC)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.21 - 1.36 g/cc
0.0437 - 0.0491 lb/in³
Average value: 1.28 g/cc Grade Count:4
Filler Content 10.0 - 40.0 %
10.0 - 40.0 %
Average value: 25.0 % Grade Count:4
Water Absorption 0.140 - 0.210 %
0.140 - 0.210 %
Average value: 0.170 % Grade Count:4
Linear Mold Shrinkage 0.000100 - 0.00200 cm/cm
0.000100 - 0.00200 in/in
Average value: 0.000875 cm/cm Grade Count:4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 93.1 - 145 MPa
13500 - 21000 psi
Average value: 122 MPa Grade Count:4
Elongation at Break 1.20 - 2.30 %
1.20 - 2.30 %
Average value: 1.73 % Grade Count:4
Modulus of Elasticity 7.65 - 24.1 GPa
1110 - 3500 ksi
Average value: 15.5 GPa Grade Count:4
Flexural Yield Strength 128 - 207 MPa
18500 - 30000 psi
Average value: 169 MPa Grade Count:4
Flexural Modulus 6.21 - 21.4 GPa
900 - 3100 ksi
Average value: 13.4 GPa Grade Count:4
Izod Impact, Notched 0.534 - 0.854 J/cm
1.00 - 1.60 ft-lb/in
Average value: 0.667 J/cm Grade Count:4
Izod Impact, Unnotched 3.20 - 3.74 J/cm
6.00 - 7.00 ft-lb/in
Average value: 3.60 J/cm Grade Count:4
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 129 - 132 °C
265 - 270 °F
Average value: 132 °C Grade Count:4
Flammability, UL94 HB
HB
Grade Count:3
Electrical Properties Metric English Comments
Electrical Resistivity 1.00 - 100 ohm-cm
1.00 - 100 ohm-cm
Average value: 25.8 ohm-cm Grade Count:4
Processing Properties Metric English Comments
Processing Temperature 202 - 249 °C
395 - 480 °F
Average value: 225 °C Grade Count:4
Mold Temperature 32.2 - 65.6 °C
90.0 - 150 °F
Average value: 48.9 °C Grade Count:4
Injection Pressure 55.2 - 82.7 MPa
8000 - 12000 psi
Average value: 68.9 MPa Grade Count:4