Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.93 - 8.40 GPa | 280 - 1220 ksi | Average value: 4.78 GPa Grade Count:10 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Modulus of Elasticity | 1.93 - 8.40 GPa | 280 - 1220 ksi | Average value: 3.06 GPa Grade Count:116 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Modulus of Elasticity | 5.30 - 8.40 GPa @Temperature 60.0 - 90.0 °C |
769 - 1220 ksi @Temperature 140 - 194 °F |
Average value: 7.70 GPa Grade Count:12 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |