Mechanical Properties Metric English Comments
Modulus of Elasticity 5.30 - 11.0 GPa
769 - 1600 ksi
Average value: 6.79 GPa Grade Count:5
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe..
Modulus of Elasticity 5.30 - 140 GPa

@Temperature -55.0 - 177 °C
769 - 20300 ksi

@Temperature -67.0 - 351 °F
Average value: 86.9 GPa Grade Count:18
Overview of materials for Epoxy/Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a..
Modulus of Elasticity 5.30 GPa
769 ksi
ISO 527
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Conditioned)
Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity.
Modulus of Elasticity 5.30 GPa
769 ksi
ISO 527-1/-2
BASF Ultramid® B3ZG6 BK 30564 30% Glass Filled PA6-1 (Conditioned)
Description: Impact-modified and 30% glass fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas..
Modulus of Elasticity 5.30 - 8.40 GPa

@Temperature 60.0 - 90.0 °C
769 - 1220 ksi

@Temperature 140 - 194 °F
Average value: 7.70 GPa Grade Count:12
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..