Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 171.1 GPa @Temperature 23.0 °C |
24820 ksi @Temperature 73.4 °F |
|
Carpenter Gall-Tough® Stainless Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1.. |
|||
Modulus of Elasticity | 171.1 GPa @Temperature 23.0 °C |
24820 ksi @Temperature 73.4 °F |
|
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 20% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |
|||
Modulus of Elasticity | 171.1 GPa @Temperature 23.0 °C |
24820 ksi @Temperature 73.4 °F |
|
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 10% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |
|||
Modulus of Elasticity | 171.1 GPa @Temperature 23.0 °C |
24820 ksi @Temperature 73.4 °F |
|
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 0% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |