Mechanical Properties Metric English Comments
Modulus of Elasticity 171.1 GPa

@Temperature 23.0 °C
24820 ksi

@Temperature 73.4 °F
Carpenter Gall-Tough® Stainless
Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1..
Modulus of Elasticity 171.1 GPa

@Temperature 23.0 °C
24820 ksi

@Temperature 73.4 °F
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 20% Cold Work
Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®..
Modulus of Elasticity 171.1 GPa

@Temperature 23.0 °C
24820 ksi

@Temperature 73.4 °F
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 10% Cold Work
Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®..
Modulus of Elasticity 171.1 GPa

@Temperature 23.0 °C
24820 ksi

@Temperature 73.4 °F
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 0% Cold Work