Mechanical Properties Metric English Comments
Modulus of Elasticity 3.40 - 12.0 GPa
493 - 1740 ksi
Average value: 6.02 GPa Grade Count:25
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Modulus of Elasticity 10.0 - 12.0 GPa
1450 - 1740 ksi
Injection; ISO 527
Raschig Group RALUPOL® 8601 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren..
Modulus of Elasticity 10.0 - 12.0 GPa
1450 - 1740 ksi
Injection; ISO 527
Raschig Group RALUPOL® 8602 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng..
Modulus of Elasticity 2.90 - 12.0 GPa
421 - 1740 ksi
Average value: 6.04 GPa Grade Count:155
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Modulus of Elasticity 3.45 - 12.0 GPa
500 - 1740 ksi
Average value: 6.11 GPa Grade Count:18
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..