Mechanical Properties Metric English Comments
Modulus of Elasticity 5.24 - 13.5 GPa
760 - 1960 ksi
Average value: 9.39 GPa Grade Count:25
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Modulus of Elasticity 4.27 - 13.5 GPa
620 - 1960 ksi
Average value: 10.5 GPa Grade Count:33
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..