Polymer Property : Modulus of Elasticity = 2.482 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.482 GPa
360.0 ksi
Kleerdex Kydex® L Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Laminating grade fire rated sheetApplications: Store fixtures and displays, exhibits, service counters, doors, partitionsFeatures: Toughness and durability, solid, integral color, chemical resistanc..
Modulus of Elasticity 2.482 GPa
360.0 ksi
KYDEX® T Acrylic/PVC Thermoplastic Sheet
Impact resistant fire rated sheetApplications: External housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for equipment such as v..
Modulus of Elasticity 2.482 GPa
360.0 ksi
Kleerdex Kydex® 510 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Weatherable and decorative sheetApplications: Housings for equipment, recreation vehicles and truck parts, safety equipment, building products, signage, wall panels, facia, doors, service counters, ..