Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

KYDEX® T Acrylic/PVC Thermoplastic Sheet

Category Polymer , Thermoplastic , Acrylic (PMMA) , Vinyl (PVC) , PVC/Acrylic Alloy
Manufacturer KYDEX LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KYDEX® T Acrylic/PVC Thermoplastic Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact resistant fire rated sheetApplications: External housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for equipment such as vending machines, air ducts, grilles, orthopedic braces, medical equipment parts, in-store displays, electrical equipment and any components requiring an UL 94 V-0 rating.Features: Kydex T is formulated to substitute for FR ABS sheet with competitive pricing but superior cost and performance. It has higher breakage resistance as measured by the Notched Izod test than competitive thermoplastics. Kydex T is available in eight gauges, in nine textures, a large variety of colors, custom blank sizes, and very low minimums. Kydex T is among the most rigid of thermoforming materials. Fabrication: Kydex T is easy to form with excellent part definition and deep-draw characteristics. It forms with similar forming times to FR-ABS making it easy transition from competitive products.Data provided by the Kleerdex Company.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 94
94
ASTM D785
Tensile Strength, Ultimate 42.0 MPa
6090 psi
ASTM D638
Elongation at Break 110 %
110 %
Modulus of Elasticity 2.482 GPa
360.0 ksi
Flexural Yield Strength 66.0 MPa
9570 psi
ASTM D790
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 75.5 °C
168 °F
annealed; ASTM D648
UL RTI, Electrical 50.0 °C

@Thickness 0.700 - 3.00 mm
122 °F

@Thickness 0.0276 - 0.118 in
UL RTI, Mechanical with Impact 50.0 °C

@Thickness 0.700 - 3.00 mm
122 °F

@Thickness 0.0276 - 0.118 in
UL RTI, Mechanical without Impact 50.0 °C

@Thickness 0.700 - 3.00 mm
122 °F

@Thickness 0.0276 - 0.118 in
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Processing Temperature 163 - 200 °C
325 - 392 °F
Forming Temperature