Mechanical Properties Metric English Comments
Modulus of Elasticity 2.557 GPa
370.9 ksi
Kleerdex Kydex® 160 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Class I/A rated thermoplastic sheetApplications: Interior ductwork and chutes, laboratory hoods, shower/tub shrouds, acoustical applications, decorative ceilings, abuse resistant surfacing for count..