Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 213.7 GPa | 31000 ksi | |
Carpenter Micro-Melt® M-4 Alloy (AISI M4) Micro-Melt® T-15 alloy is a high-carbon tungsten-cobalt-vanadium high speed powder metal. This grade possesses very high wear resistance coupled with high strength. The advantages of Micro-Melt pre.. |