Carpenter Micro-Melt® M-4 Alloy (AISI M4)

Category Metal , Ferrous Metal , Carbon Steel , High Carbon Steel , Tool Steel
Manufacturer Carpenter Technology Corporation (Cartech)
Trade Name Micro-Melt®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carpenter Micro-Melt® M-4 Alloy (AISI M4).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Micro-Melt® T-15 alloy is a high-carbon tungsten-cobalt-vanadium high speed powder metal. This grade possesses very high wear resistance coupled with high strength. The advantages of Micro-Melt premium powder high speed steels include ease of grinding, response to heat treatment, more uniform structure, greater wear resistance and improved toughness. In addition, Carpenter's unique hot rolling and rotary forging capabilities impart minimal distortion characteristics to these alloys. Micro-Melt M-4 alloy changes size only slightly after hardening. A 1" cube will expand about 0.0005" in hardening at 2225°F and will expand a like amount when tempered at 1050°F.Applications: Lathe tools, Planer tools, Drills, Taps, Reamers, Broaches, Milling cutters, Form cutters, Thread chasers, Hobs, Counterbores, Inserts-heading diesInformation provided by Carpenter Technology Corporation.Micro-Melt® is a registered trademark of Carpenter Technology Corporation.
Physical Properties Metric English Comments
Specific Gravity 7.97 g/cc
7.97 g/cc
Mechanical Properties Metric English Comments
Hardness, Rockwell C 64 - 65
64 - 65
As hardened
66
66
Tempered 2 hours at 1000°F
Modulus of Elasticity 213.7 GPa
31000 ksi
Thermal Properties Metric English Comments
CTE, linear 9.56 µm/m-°C

@Temperature 37.8 - 260 °C
5.31 µin/in-°F

@Temperature 100 - 500 °F
11.95 µm/m-°C

@Temperature 37.8 - 538 °C
6.639 µin/in-°F

@Temperature 100 - 1000 °F
12.6 µm/m-°C

@Temperature 37.8 - 816 °C
7.00 µin/in-°F

@Temperature 100 - 1500 °F
Component Elements Properties Metric English Comments
Carbon, C 1.35 %
1.35 %
Chromium, Cr 4.5 %
4.5 %
Iron, Fe 79.49 %
79.49 %
As Balance
Manganese, Mn 0.30 %
0.30 %
Molybdenum, Mo 4.5 %
4.5 %
Silicon, Si 0.30 %
0.30 %
Sulfur, S 0.060 %
0.060 %
Tungsten, W 5.5 %
5.5 %
Vanadium, V 4.0 %
4.0 %