Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 16.1 - 150 GPa

@Temperature -55.0 - 332 °C
2340 - 21800 ksi

@Temperature -67.0 - 630 °F
Average value: 69.2 GPa Grade Count:2
Overview of materials for Polyimide
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..