Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 16.1 - 150 GPa @Temperature -55.0 - 332 °C |
2340 - 21800 ksi @Temperature -67.0 - 630 °F |
Average value: 69.2 GPa Grade Count:2 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |