Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 22.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 22.0 GPa
3190 ksi
Lehmann & Voss LUVOCOM® 19/CF/30 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Modulus of Elasticity 22.0 GPa
3190 ksi
Young's modulus
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride
Boralloy® Pyrolytic Boron Nitride (PBN) is an anisotropic, high-temperature ceramic which exhibits a unique combination of high electrical resistance and good thermal conductivity. This non-toxi..
Modulus of Elasticity 22.0 GPa
3190 ksi
Lehmann & Voss LUVOCOM® 1105-7141 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolys..
Modulus of Elasticity 22.0 GPa
3190 ksi
25mm flat samples, compression moulded; ISO 527-4
Menzolit Menzolit® HPC 1200 Unsaturated Polyester UP
HPC 1200 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc..
Modulus of Elasticity 22.0 GPa
3190 ksi
Lehmann & Voss LUVOCOM® 1-0890 Polyamide 66, with carbon fiber, low-warpage, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c..
Modulus of Elasticity 22.0 GPa
3190 ksi
0° Fiber Direction; In Tension
Saint-Gobain Quartzel® Fabric/Cyanate Ester Resin Composite
Fiber: Quartzel® 8 Harness Fabric Style 581. Resin 954-2A System.Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, n..
Modulus of Elasticity 22.0 GPa

@Thickness >=1.50 mm
3190 ksi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t..
Modulus of Elasticity 22.0 GPa

@Thickness >=1.50 mm
3190 ksi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2
Elektro-Isola G-Etronax EP 215 S Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic temperatures. Very good where t..
Modulus of Elasticity 22.0 GPa

@Thickness >=1.50 mm
3190 ksi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. UL-94 V..
Modulus of Elasticity 22.0 GPa

@Thickness >=1.50 mm
3190 ksi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c..
Modulus of Elasticity 22.0 GPa

@Thickness >=1.50 mm
3190 ksi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2
Elektro-Isola G-Etronax EP 203 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c..
Modulus of Elasticity 22.0 GPa
3190 ksi
Young's modulus
Momentive Performance Materials Pyrolytic Boron Nitride (PBN) Coating
High temperature protective coating for graphite.PBN has become the material of choice for compound semiconductor crystal growth and wafer processing. PBN coatings also seal and protect graphite fr..
Modulus of Elasticity 22.0 GPa
3190 ksi
Lehmann & Voss LUVOCOM® 1105-8165 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Electrically c..