Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 221 GPa | 32100 ksi | RT |
Haynes 263® alloy, cold rolled sheet, solution treated and aged Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle.. |
|||
Modulus of Elasticity | 221 GPa | 32000 ksi | |
Latrobe DuraTechâ„¢ NINE Powder Metal Tool Steel DuraTech NINE is an air-hardening, powder metal tool steel that provides very high wear resistance in combination with high impact toughness. A large volume of hard vanadium carbides provides the hi.. |
|||
Modulus of Elasticity | 221 GPa | 32100 ksi | ASTM C848 |
CoorsTek AD-85 Alumina (nom. 85% Al2O3) Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Modulus of Elasticity | 221 GPa | 32100 ksi | |
Crucible Steel CPM® 10V® (AISI A11) Tool Steel CPM 10V was the first in the family of high vanadium tool steels made by the Crucible Particle Metallurgy process. Crucible engineers optimized the vanadium content to provide superior wear resistan.. |
|||
Modulus of Elasticity | 221 GPa | 32100 ksi | |
Crucible Steel CPM® 9V® Tool Steel CPM 9V is made by the Crucible Particle Metallurgy process. Its composition is a modification of CPM 10V with lower carbon and vanadium to improve toughness and heat check resistance. These enhanced.. |
|||
Modulus of Elasticity | 221 GPa | 32100 ksi | |
Crucible Steel CPM® S30V® Stainless Steel CPM S30V is a martensitic stainless steel designed to offer the best combination of toughness, wear resistance and corrosion resistance. Its chemistry has been specially balanced to promote the form.. |
|||
Modulus of Elasticity | 221 GPa | 32100 ksi | |
Crucible Steel CPM® S35VN™ Stainless Steel CPM S35VN is a martensitic stainless steel designed to offer improved toughness over CPM S30V. It is also easier to machine and polish than CPM S30V. Its chemistry has been rebalanced so that it for.. |
|||
Modulus of Elasticity | 221 GPa | 32100 ksi | |
Bohler-Uddeholm BÖHLER K294 MICROCLEAN AISI A11 Powder Metal Tool Steel Properties: Powder-metallurgical produced cold work tool steel with extremely high wear resistance, good toughness and high compressive strength. The latest generation of powder metal technology ena.. |
|||
Modulus of Elasticity | 221 GPa @Temperature 399 °C |
32000 ksi @Temperature 750 °F |
hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel Uddeholm Vanadis 60 is a high alloyed powder metallurgical high speed steel suitable for very demanding cold work applications and for cutting tools. The high carbon and alloying content, Co, Mo, W .. |
|||
Modulus of Elasticity | 221 GPa | 32000 ksi | |
California Fine Wire Alloy 422 Precious Metal Alloy All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Modulus of Elasticity | 221 GPa | 32000 ksi | |
Latrobe DuraTech™ A11 Powder Metal Tool Steel (AISI A11) DuraTech A11 powder metal tool steel a versatile air-hardening tool and die steel which provides extremely high wear resistance in combination with relatively high impact toughness. A very large vol.. |