Crucible Steel CPM® 9V® Tool Steel

Category Metal , Ferrous Metal , Carbon Steel , High Carbon Steel , Tool Steel
Manufacturer Crucible Steel
Trade Name CPM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Steel CPM® 9V® Tool Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CPM 9V is made by the Crucible Particle Metallurgy process. Its composition is a modification of CPM 10V with lower carbon and vanadium to improve toughness and heat check resistance. These enhanced properties permit CPM 9V to perform well in problem applications where high carbon, high chromium tool steels, such as CPM 10V or the high speed steels, lack sufficient toughness or heat check resistance, or where lower alloy tool steels and hot work tool steels lack sufficient wear resistance.The CPM process produces very homogeneous, high quality steel characterized by superior dimensional stability, grindability, and toughness compared to steels produced by conventional processes.Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Density 7.455 g/cc
0.2693 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 223 - 255
223 - 255
Annealed
Hardness, Rockwell C 54 - 56
54 - 56
Modulus of Elasticity 221 GPa
32100 ksi
Flexural Strength 4136 MPa
599900 psi
Hardening Temperature- 1120°C, Tempering Temperature- 540°C
4177 MPa
605800 psi
Hardening Temperature- 1175°C, Tempering Temperature- 550°C
Charpy Impact 35.0 J
25.8 ft-lb
Hardening Temperature- 1175°C; Tempering Temperature- 550°C
63.0 J
46.5 ft-lb
Hardening Temperature- 1120°C; Tempering Temperature- 540°C
99.0 J
73.0 ft-lb
Hardening Temperature- 1065°C; Tempering Temperature- 595°C
Thermal Properties Metric English Comments
CTE, linear 11.07 µm/m-°C

@Temperature 20.0 - 90.0 °C
6.150 µin/in-°F

@Temperature 68.0 - 194 °F
11.18 µm/m-°C

@Temperature 20.0 - 200 °C
6.211 µin/in-°F

@Temperature 68.0 - 392 °F
11.61 µm/m-°C

@Temperature 20.0 - 430 °C
6.450 µin/in-°F

@Temperature 68.0 - 806 °F
Thermal Conductivity 20.48 W/m-K
142.1 BTU-in/hr-ft²-°F
21.6 W/m-K

@Temperature 100 °C
150 BTU-in/hr-ft²-°F

@Temperature 212 °F
25.25 W/m-K

@Temperature 300 °C
175.2 BTU-in/hr-ft²-°F

@Temperature 572 °F
25.81 W/m-K

@Temperature 500 °C
179.1 BTU-in/hr-ft²-°F

@Temperature 932 °F
26.08 W/m-K

@Temperature 540 °C
181.0 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Component Elements Properties Metric English Comments
Carbon, C 1.9 %
1.9 %
Chromium, Cr 5.25 %
5.25 %
Iron, Fe 82.45 %
82.45 %
As Remainder
Molybdenum, Mo 1.3 %
1.3 %
Vanadium, V 9.1 %
9.1 %