Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.185 GPa | 26.8 ksi | Molded Sample 2% Secant Modulus |
Dow LDPE 779I Low Density Polyethylene DOW LDPE 779I resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent rigidity. Typical applications include caps.. |
|||
Modulus of Elasticity | 0.185 - 1.80 GPa | 26.8 - 261 ksi | Average value: 1.08 GPa Grade Count:30 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |