Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.00 - 1.05 g/cc
0.0361 - 0.0379 lb/in³
Average value: 1.03 g/cc Grade Count:36
Water Absorption 0.230 - 1.90 %
0.230 - 1.90 %
Average value: 1.26 % Grade Count:19
Moisture Absorption at Equilibrium 0.750 - 1.10 %
0.750 - 1.10 %
Average value: 0.943 % Grade Count:7
Linear Mold Shrinkage 0.00400 - 0.0180 cm/cm
0.00400 - 0.0180 in/in
Average value: 0.0126 cm/cm Grade Count:4
Melt Flow 0.800 - 56.0 g/10 min
0.800 - 56.0 g/10 min
Average value: 16.7 g/10 min Grade Count:18
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105 - 110
105 - 110
Average value: 107 Grade Count:6
Tensile Strength, Ultimate 40.0 - 68.9 MPa
5800 - 10000 psi
Average value: 52.3 MPa Grade Count:14
Tensile Strength, Yield 15.0 - 44.0 MPa
2180 - 6380 psi
Average value: 35.1 MPa Grade Count:25
Elongation at Break 10.0 - 400 %
10.0 - 400 %
Average value: 126 % Grade Count:37
Elongation at Yield 5.00 - 42.0 %
5.00 - 42.0 %
Average value: 17.1 % Grade Count:24
Modulus of Elasticity 0.185 - 1.80 GPa
26.8 - 261 ksi
Average value: 1.08 GPa Grade Count:30
Flexural Yield Strength 51.7 - 89.6 MPa
7500 - 13000 psi
Average value: 77.0 MPa Grade Count:3
Flexural Modulus 0.380 - 1.38 GPa
55.1 - 200 ksi
Average value: 0.985 GPa Grade Count:11
Izod Impact, Notched 0.400 - 8.01 J/cm
0.749 - 15.0 ft-lb/in
Average value: 2.40 J/cm Grade Count:9
0.260 - 0.260 J/cm

@Temperature -40.0 - -40.0 °C
0.487 - 0.487 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.260 J/cm Grade Count:1
Izod Impact, Unnotched 6.41 - 5340 J/cm
12.0 - 10000 ft-lb/in
Average value: 6.41 J/cm Grade Count:3
Charpy Impact Unnotched 1000 J/cm² - NB
4760 ft-lb/in² - NB
Grade Count:19
999.9 - 999.9 J/cm²

@Temperature -30.0 - -30.0 °C
4759 - 4759 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Grade Count:2
Charpy Impact, Notched 0.730 J/cm² - NB
3.47 ft-lb/in² - NB
Average value: 1.88 J/cm² Grade Count:18
0.490 - 2.42 J/cm²

@Temperature -30.0 - -30.0 °C
2.33 - 11.5 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.17 J/cm² Grade Count:18
Thermal Properties Metric English Comments
CTE, linear 85.0 - 120 µm/m-°C
47.2 - 66.7 µin/in-°F
Average value: 96.4 µm/m-°C Grade Count:14
Thermal Conductivity 0.230 - 0.346 W/m-K
1.60 - 2.40 BTU-in/hr-ft²-°F
Average value: 0.276 W/m-K Grade Count:4
Melting Point 175 - 191 °C
347 - 376 °F
Average value: 183 °C Grade Count:31
Maximum Service Temperature, Air 80.0 - 150 °C
176 - 302 °F
Average value: 103 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 70.0 - 150 °C
158 - 302 °F
Average value: 140 °C Grade Count:20
Deflection Temperature at 1.8 MPa (264 psi) 40.0 - 55.0 °C
104 - 131 °F
Average value: 49.8 °C Grade Count:24
Vicat Softening Point 140 - 160 °C
284 - 320 °F
Average value: 154 °C Grade Count:11
Flammability, UL94 HB - V-2
HB - V-2
Grade Count:22
Oxygen Index 22.0 - 25.0 %
22.0 - 25.0 %
Average value: 24.0 % Grade Count:3
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+11 - 2.00e+15 ohm-cm
1.00e+11 - 2.00e+15 ohm-cm
Average value: 2.79e+14 ohm-cm Grade Count:13
Surface Resistance 5.00e+11 - 1.00e+14 ohm
5.00e+11 - 1.00e+14 ohm
Average value: 6.72e+13 ohm Grade Count:9
Dielectric Constant 3.10 - 4.00
3.10 - 4.00
Average value: 3.55 Grade Count:4
Dielectric Strength 19.7 - 40.0 kV/mm
500 - 1020 kV/in
Average value: 29.2 kV/mm Grade Count:13
Dissipation Factor 0.000325 - 0.0500
0.000325 - 0.0500
Average value: 0.00538 Grade Count:7
Comparative Tracking Index 600 V
600 V
Average value: 600 V Grade Count:6
Processing Properties Metric English Comments
Processing Temperature 216 - 282 °C
420 - 540 °F
Average value: 251 °C Grade Count:3
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Average value: 49.4 °C Grade Count:4
Drying Temperature 79.4 - 80.0 °C
175 - 176 °F
Average value: 79.8 °C Grade Count:3
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:3