Polymer Property : Modulus of Elasticity = 276 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 276 GPa
40000 ksi
Hogen HM1000 Tungsten-Based Metal
Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offe..
Modulus of Elasticity 276 GPa
40000 ksi
Mi-Tech Metals HD17 Tungsten-Based Metal
Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; ASTM B-777-07 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Nil magnetic properties.Manufactured by powder metallurgy methods. ..
Modulus of Elasticity 276 GPa
40000 ksi
Mi-Tech Metals HD17BB Tungsten-Based Metal
ASTM B-777-07 Class 1; Slightly Magnetic (HD17 is non-magnetic).Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist t..
Modulus of Elasticity 276 GPa
40000 ksi
Tensile modulus calculated at secant 6000-1000
Hexcel® IM4 Carbon Fiber (12,000 Filaments)
Weight/length = 0.723 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Modulus of Elasticity 276 GPa
40000 ksi
Tensile modulus calculated at secant 6000-1000
Hexcel® IM6 Carbon Fiber (12,000 Filaments)
Weight/length = 0.446 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Modulus of Elasticity 276 GPa
40000 ksi
Tensile modulus calculated at secant 6000-1000
Hexcel® IM7 Carbon Fiber (12,000 Filaments)
Weight/length = 0.446 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Modulus of Elasticity 276 GPa
40000 ksi
Tensile modulus calculated at secant 6000-1000
Hexcel® IM7 Carbon Fiber (6000 Filaments)
Weight/length = 0.223 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Modulus of Elasticity 276 GPa
40000 ksi
Tensile modulus calculated at secant 6000-1000
Hexcel® IM9 Carbon Fiber (12,000 Filaments)
Weight/length = 0.331 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Modulus of Elasticity 276 GPa
40000 ksi
ASTM C848
CoorsTek AD-90 Alumina (nom. 90% Al2O3)
Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Modulus of Elasticity 276 GPa
40000 ksi
At 55° to rolling direction
AK Steel TRAN-COR® H-0 CARLITE® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Modulus of Elasticity 276 GPa
40000 ksi
At 55° to rolling direction
AK Steel TRAN-COR® H-1 CARLITE® DR® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Modulus of Elasticity 276 GPa
40000 ksi
At 55° to rolling direction
AK Steel TRAN-COR® H-1 CARLITE® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Modulus of Elasticity 276 GPa
40000 ksi
At 55° to rolling direction
AK Steel TRAN-COR® H-2 CARLITE® DR® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Modulus of Elasticity 276 GPa
40000 ksi
At 55° to rolling direction
AK Steel TRAN-COR® H-2 CARLITE® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Modulus of Elasticity 276 GPa
40000 ksi
At 55° to rolling direction
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..