Mechanical Properties Metric English Comments
Modulus of Elasticity 3.40 - 29.0 GPa

@Temperature -40.0 - 250 °C
493 - 4210 ksi

@Temperature -40.0 - 482 °F
Average value: 12.3 GPa Grade Count:3
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Modulus of Elasticity 3.40 - 29.0 GPa

@Thickness 1.60 - 3.17 mm
493 - 4210 ksi

@Thickness 0.0630 - 0.125 in
Average value: 12.3 GPa Grade Count:3
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Modulus of Elasticity 4.50 - 29.0 GPa
653 - 4200 ksi
Average value: 16.5 GPa Grade Count:8
Overview of materials for Thermoplastic Polyimide, Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va..
Modulus of Elasticity 10.3 - 29.0 GPa
1490 - 4210 ksi
Average value: 15.2 GPa Grade Count:8
Overview of materials for Phenolic, Novolac, Mineral/Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Graphite Filled". Each property range of values reported is minimum and maxim..
Modulus of Elasticity 1.60 - 29.0 GPa
232 - 4200 ksi
Average value: 8.94 GPa Grade Count:55
Overview of materials for Polytrimethylene Terephthalate (PTT)
This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val..