Polymer Property : Modulus of Elasticity = 290 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 290 - 310 GPa
42100 - 45000 ksi
Youngs Modulus
MMCC Al/Al2O3 Continuous Fiber Aluminum Matrix Composite
Cast, reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
Modulus of Elasticity 290 GPa
42100 ksi
H.C. Starck WCu 85/15 Tungsten-Copper Composite Material
Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm..
Modulus of Elasticity 290 GPa
42100 ksi
In Tension
Cytec Thornel® T-40 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..
Modulus of Elasticity 290 GPa
42100 ksi
In Tension
Cytec Thornel® T-650/42 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..
Modulus of Elasticity 290 GPa
42100 ksi
In Tension
Cytec Thornel® T-650/42 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..